Can you specife some result from your test´s. I gues that what i´m looking for is what type of increase you get swithing from plate´s to mesh and is it the same mas?
In my world mas is equel to recistance, so the lower mas the lower recistance, and lower resistance is lower amp. I just don´t understand way some people are using plate´s that are 1-1.5 mm, after all, it is on the surfuce the action is. I use 0,3 mm and that works fine
My next cell is made of mesh electrodes x 30 cells. Stainless anodes and titanium coated cooper katodes. The process of coating the cooper are done by a friend, he knows how it´s done, and i´m looking forward to the resulte.Statistics: Posted by Hydrogenworld — Fri Apr 04, 2008 10:39 pm
]]>